Casting Alloys
 

White Metal Alloys for  Jewelry & Pewter Making

     
  For all of your centrifugical spin casting alloys, gravity pour alloys & pewter alloys.

At Alchemy, we produce hundreds of different alloys.  Our alloys are used in many different applications, such as: 

Costume jewelry, fishing, medallions, trophies, belt buckles, silverware, pewter-ware, figurines, toy soldiers, to name a few.

Small Order Pricing

     

Available in the following Bars Sizes:

1.75Lb Cast Bar - ** Most Popular **

8Lb Nolan Bar

 

     

ARE YOU NEW TO THE HOBBY AND WANT HELP PICKING AN ALLOY?

Try these Lead-Free Alloys: BM91, LOW 281, 97SP

 

 LEAD-FREE ALLOYS

 
 LOW 281 (Lead-Free)    #908 (Lead-Free)
 COMPOSITION: Tin (Sn) 42%    COMPOSITION: Tin (Sn) 90%
Bismuth (Bi) 58%   Antimony (Sb) 8%
    Copper (Cu) 2%

 Density: 0.3090 Lbs/in3 (8.56 g/cm3)

 

 Density: 0.2626 Lbs/in3 (7.27 g/cm3)

 Casting Temp: 300-400oF (149-203oC)    Casting Temp: 500-550oF (260-288oC)

 Recommended Use

 

 Recommended Use

 ● General Casting Most Products    ● Hard Surface/Tailored Pieces

 Industry Equivalents

 

 Industry Equivalents

 ● AIM 138, Cerrotru    ● Atlas 7902
         
 BM91 (Lead-Free)  

 #927 (Lead-Free)

 COMPOSITION: Tin (Sn) 91%    COMPOSITION: Tin (Sn) 92%
Antimony (Sb) 8%   Antimony (Sb) 7%
Copper (Cu) 1%   Copper (Cu) 1%
 Density: 0.2620 Lbs/in3 (7.25 g/cm3)  

 Density: 0.2622 Lbs/in3 (7.26 g/cm3)

 Casting Temp: 500-550oF (260-288oC)    Casting Temp: 500-550oF (260-288oC)
 Recommended Use  

 Recommended Use

 ● General Casting Most Products    ● Excellent for large intricate castings
 Industry Equivalents  

 Industry Equivalents

 ● CMC BM91    ● Hirsch CP2
 
 R8 (Lead-Free)  

 BR5 (Lead-Free)

 COMPOSITION: Tin (Sn) 92%    COMPOSITION: Tin (Sn) 92%
Antimony (Sb) 7.5%   Antimony (Sb) 7.75%
Copper (Cu) 0.5%   Copper (Cu) 0.25%
 Density: 0.2620 Lbs/in3 (7.25 g/cm3)  

 Density: 0.2616 Lbs/in3 (7.24 g/cm3)

 Casting Temp: 500-550oF (260-288oC)    Casting Temp: 500-550oF (260-288oC)
 Recommended Use  

 Recommended Use

 ● General Casting Most Products    ● Hard Surface/Tailored Pieces
 Industry Equivalents  

 Industry Equivalents

 ● AIM 92(R8)    ● Atlas 7921, Conquest NC-BR5, Hirsch CP1
         
 BM92 (Lead-Free)  

 BM94 (Lead-Free)

 COMPOSITION: Tin (Sn) 92%    COMPOSITION: Tin (Sn) 94%
Antimony (Sb) 8%   Antimony (Sb) 5%
    Copper (Cu) 1%
 Density: 0.2614 Lbs/in3 (7.24 g/cm3)  

 Density: 0.2626 Lbs/in3 (7.27 g/cm3)

 Casting Temp: 500-550oF (260-288oC)    Casting Temp: 500-550oF (260-288oC)
 Recommended Use  

 Recommended Use

 ● Excellent for large intricate castings    ● Semi-Tailored Pieces
 Industry Equivalents  

 Industry Equivalents

 ● Canfield J-592, Conquest NC-92, Hirsch CP    ● CMC BM94
         
 #954 (Lead-Free)  

 97SP (Lead-Free)

 COMPOSITION: Tin (Sn) 95%    COMPOSITION: Tin (Sn) 97%
Antimony (Sb) 3.8%   Bismuth (Bi) 2.5%
Copper (Cu) 1.2%   Copper (Cu) 0.5%
 Density: 0.2631 Lbs/in3 (7.28 g/cm3)  

 Density: 0.2659 Lbs/in3 (7.36 g/cm3)

 Casting Temp: 500-550oF (260-288oC)    Casting Temp: 500-550oF (260-288oC)
 Recommended Use  

 Recommended Use

 ● Semi-Tailored Pieces    ● General Casting Most Products
 Industry Equivalents  

 Industry Equivalents

 ● AIM 95, Canfield J-95    ● AIM 97SP
         

 97SA (Lead-Free)

   #981 (Lead-Free)
 COMPOSITION: Tin (Sn) 97%    COMPOSITION: Tin (Sn) 98%
Bismuth (Bi) 2.5%   Antimony (Sb) 1%
Silver (Ag) 0.5%   Bismuth (Bi) 1%

 Density: 0.2660 Lbs/in3 (7.37 g/cm3)

   Density: 0.2640 Lbs/in3 (7.31 g/cm3)
 Casting Temp: 500-550oF (260-288oC)    Casting Temp: 550-600oF (288-316oC)

 Recommended Use

   Recommended Use
 ● General Casting Most Products    ● Good Dapping Qualities

 Industry Equivalents

   Industry Equivalents
 ● AIM 97SA    ● AIM 98NL
         

LEAD BASED ALLOYS

 

 SB03

   SB04
 COMPOSITION: Antimony (Sb) 3%    COMPOSITION: Antimony (Sb) 4%
Lead (Pb) 97%   Lead (Pb) 96%
     

 Density: 0.4041 Lbs/in3 (11.21 g/cm3)

   Density: 0.4024 Lbs/in3 (11.16 g/cm3)
 Casting Temp: 750-850oF (399-454oC)    Casting Temp: 750-850oF (399-454oC)

 Recommended Use

   Recommended Use
 ● Inexpensive alloy for key chains,     counterweights, fishing lures, giveaways.    ● Inexpensive alloy for key chains,  counterweights, fishing lures, giveaways.

 Industry Equivalents

   Industry Equivalents
 ● Machine Lead    ● Hirsch 4AL
         

 J104

   J105
 COMPOSITION: Tin (Sn) 1%    COMPOSITION: Tin (Sn) 1%
Antimony (Sb) 4.5%   Antimony (Sb) 4.75%
Lead (Pb) 94.5%   Lead (Pb) 94.25%

 Density: 0.4001 Lbs/in3 (11.10 g/cm3)

   Density: 0.3997 Lbs/in3 (11.08 g/cm3)
 Casting Temp: 700-800oF (371-427oC)    Casting Temp: 700-800oF (371-427oC)

 Recommended Use

   Recommended Use
 ● Inexpensive alloy for key chains, giveaways.    ● Inexpensive alloy for key chains, giveaways.

 Industry Equivalents

   Industry Equivalents
 ● Canfield J-104    ● Canfield J-105
         

 SB06

   J106
 COMPOSITION: Antimony (Sb) 6%    COMPOSITION: Tin (Sn) 1%
Lead (Pb) 94%   Antimony (Sb) 6%
    Lead (Pb) 93%

 Density: 0.3990 Lbs/in3 (11.07 g/cm3)

   Density: 0.3975 Lbs/in3 (11.03 g/cm3)
 Casting Temp: 750-850oF (399-454oC)    Casting Temp: 700-800oF (371-427oC)

 Recommended Use

   Recommended Use
 ● Belt Buckles, Bulky items    ● Inexpensive alloy for key chains, giveaways.

 Industry Equivalents

   Industry Equivalents
 ● Hirsch AL6    ● Canfield J-106, Hirsch B1
         

 SB10

   SB12
 COMPOSITION: Antimony (Sb) 10%    COMPOSITION: Antimony (Sb) 12%
Lead (Pb) 90%   Lead (Pb) 88%
     

 Density: 0.3922 Lbs/in3 (10.88 g/cm3)

   Density: 0.3888 Lbs/in3 (10.78 g/cm3)
 Casting Temp: 750-850oF (399-454oC)    Casting Temp: 750-850oF (399-454oC)

 Recommended Use

   Recommended Use
 ● Trophies, Statues    ● Trophies, Statues

 Industry Equivalents

   Industry Equivalents
 ● Hirsch 10AL    ● Hirsch 12AL
         

 CT Metal

   2/6 Alloy
 COMPOSITION: Tin (Sn) 1%    COMPOSITION: Tin (Sn) 2%
Antimony (Sb) 13%   Antimony (Sb) 6%
Lead (Pb) 86%   Lead (Pb) 92%

 Density: 0.3856 Lbs/in3 (10.69 g/cm3)

   Density: 0.3961 Lbs/in3 (10.99 g/cm3)
 Casting Temp: 700-800oF (371-427oC)    Casting Temp: 700-800oF (371-427oC)

 Recommended Use

   Recommended Use
 ● Casket Trim, Trophies, Statues    ● Decorative, Flatware, Belt buckles.

 Industry Equivalents

   Industry Equivalents
 ● AIM CT, Hirsch CT    ● AIM 2S
         

 2/8 Alloy

   3/8 Alloy
 COMPOSITION: Tin (Sn) 2%    COMPOSITION: Tin (Sn) 3%
Antimony (Sb) 8%   Antimony (Sb) 8%
Lead (Pb) 90%   Lead (Pb) 89%

 Density: 0.3927 Lbs/in3 (10.89 g/cm3)

   Density: 0.3912 Lbs/in3 (10.85 g/cm3)
 Casting Temp: 700-800oF (371-427oC)    Casting Temp: 700-800oF (371-427oC)

 Recommended Use

   Recommended Use
 ● Decorative, Flatware, Belt buckles.    ● Decorative, Flatware, Belt buckles.

 Industry Equivalents

   Industry Equivalents
 ● Hirsch B4    ● Canfield J-308, Hirsch B3
         

 3/10 Alloy

   Electrotype
 COMPOSITION: Tin (Sn) 3%    COMPOSITION: Tin (Sn) 3.5%
Antimony (Sb) 10%   Antimony (Sb) 3.5%
Lead (Pb) 87%   Lead (Pb) 93%

 Density: 0.3878 Lbs/in3 (10.76 g/cm3)

   Density: 0.3981 Lbs/in3 (11.04 g/cm3)
 Casting Temp: 700-800oF (371-427oC)    Casting Temp: 700-800oF (371-427oC)

 Recommended Use

   Recommended Use
 ● Decorative, Flatware, Belt buckles.    ● Decorative, Flatware, Belt buckles.

 Industry Equivalents

   Industry Equivalents
 ● Atlas 5877    ● CMC Electrotype
         

 4/6 Alloy

   #10 Linotype
 COMPOSITION: Tin (Sn) 4%    COMPOSITION: Tin (Sn) 4%
Antimony (Sb) 6%   Antimony (Sb) 12%
Lead (Pb) 90%   Lead (Pb) 84%

 Density: 0.3932 Lbs/in3 (10.90 g/cm3)

   Density: 0.3830 Lbs/in3 (10.62 g/cm3)
 Casting Temp: 700-800oF (371-427oC)    Casting Temp: 700-800oF (371-427oC)

 Recommended Use

   Recommended Use
 ● Decorative, Flatware, Belt buckles.    ● Decorative, Flatware, Belt buckles.

 Industry Equivalents

   Industry Equivalents
 ● Conquest NC-3    ● Atlas 5841
         

 5/5 Alloy

   5/15 Monotype
 COMPOSITION: Tin (Sn) 5%    COMPOSITION: Tin (Sn) 5%
Antimony (Sb) 5%   Antimony (Sb) 15%
Lead (Pb) 90%   Lead (Pb) 80%

 Density: 0.3934 Lbs/in3 (10.91 g/cm3)

   Density: 0.3764 Lbs/in3 (10.44 g/cm3)
 Casting Temp: 700-800oF (371-427oC)    Casting Temp: 700-800oF (371-427oC)

 Recommended Use

   Recommended Use
 ● Decorative, Flatware, Belt buckles.    ● Decorative, Flatware, Belt buckles.

 Industry Equivalents

   Industry Equivalents
 ● Hirsch B5    ● CMC 5/15 Monotype
         

 6/8 Toning

   10/11 Toning
 COMPOSITION: Tin (Sn) 6%    COMPOSITION: Tin (Sn) 10%
Antimony (Sb) 8%   Antimony (Sb) 11%
Lead (Pb) 86%   Lead (Pb) 79%

 Density: 0.3868 Lbs/in3 (10.73 g/cm3)

   Density: 0.3759 Lbs/in3 (10.42 g/cm3)
 Casting Temp: 700-800oF (371-427oC)    Casting Temp: 700-800oF (371-427oC)

 Recommended Use

   Recommended Use
 ● Decorative, Flatware, Belt buckles.    ● Novelty.

 Industry Equivalents

   Industry Equivalents
  CMC 6/8 Toning     CMC 10/11 Toning
         

 #11

   #16
 COMPOSITION: Tin (Sn) 11%    COMPOSITION: Tin (Sn) 16%
Antimony (Sb) 2%   Antimony (Sb) 3%
Lead (Pb) 87%   Lead (Pb) 81%

 Density: 0.3897 Lbs/in3 (10.81 g/cm3)

   Density: 0.3808 Lbs/in3 (10.56 g/cm3)
 Casting Temp: 700-800oF (371-427oC)    Casting Temp: 600-700oF (316-371oC)

 Recommended Use

   Recommended Use
 ● Novelty.    ● Novelty.

 Industry Equivalents

   Industry Equivalents
 ● Conquest N-11    ● AIM 16
         

 #164

   #204
 COMPOSITION: Tin (Sn) 16%    COMPOSITION: Tin (Sn) 20%
Antimony (Sb) 4%   Antimony (Sb) 4%
Lead (Pb) 80%   Lead (Pb) 76%

 Density: 0.3791 Lbs/in3 (10.51 g/cm3)

   Density: 0.3732 Lbs/in3 (10.35 g/cm3)
 Casting Temp: 600-700oF (316-371oC)    Casting Temp: 600-700oF (316-371oC)

 Recommended Use

   Recommended Use
 ● Novelty.    ● Novelty.

 Industry Equivalents

   Industry Equivalents
 ● Hirsch 164    ● Hirsch 204
         

 J32

   #251
 COMPOSITION: Tin (Sn) 23%    COMPOSITION: Tin (Sn) 25%
Antimony (Sb) 2%   Antimony (Sb) 1%
Lead (Pb) 75%   Lead (Pb) 74%

 Density: 0.3722 Lbs/in3 (10.32 g/cm3)

   Density: 0.3710 Lbs/in3 (10.29 g/cm3)
 Casting Temp: 575-675oF (302-357oC)    Casting Temp: 575-675oF (302-357oC)

 Recommended Use

   Recommended Use
 ● Novelty.    ● Novelty.

 Industry Equivalents

   Industry Equivalents
 ● Canfield J-32    ● Conquest NC-25S
         

 25LC

   #253
 COMPOSITION: Tin (Sn) 25%    COMPOSITION: Tin (Sn) 25%
Antimony (Sb) 3%   Antimony (Sb) 3%
Lead (Pb) 71%   Lead (Pb) 72%
Cadmium (Cd) 1%    

 Density: 0.3667 Lbs/in3 (10.17 g/cm3)

   Density: 0.3676 Lbs/in3 (10.19 g/cm3)
 Casting Temp: 575-675oF (302-357oC)    Casting Temp: 575-675oF (302-357oC)

 Recommended Use

   Recommended Use
 ● Novelty.    ● Novelty.

 Industry Equivalents

   Industry Equivalents
 ● AIM 25LC    ● Canfield J-253, Hirsch 253
         

 #283

   #32
 COMPOSITION: Tin (Sn) 28%    COMPOSITION: Tin (Sn) 32%
Antimony (Sb) 3%   Antimony (Sb) 3%
Lead (Pb) 69%   Lead (Pb) 65%

 Density: 0.3632 Lbs/in3 (10.07 g/cm3)

   Density: 0.3574 Lbs/in3 (9.91 g/cm3)
 Casting Temp: 575-675oF (302-357oC)    Casting Temp: 575-675oF (302-357oC)

 Recommended Use

   Recommended Use
 ● Novelty.    ● Soft Boutique.

 Industry Equivalents

   Industry Equivalents
 ● Hirsch 283    ● Aim 32, Canfield J-323, Conquest NC-32,    Hirsch 32
         

 #35

   36A
 COMPOSITION: Tin (Sn) 35%    COMPOSITION: Tin (Sn) 36%
Antimony (Sb) 3%   Antimony (Sb) 2%
Lead (Pb) 62%   Lead (Pb) 62%

 Density: 0.3530 Lbs/in3 (9.79 g/cm3)

   Density: 0.3533 Lbs/in3 (9.79 g/cm3)
 Casting Temp: 575-675oF (302-357oC)    Casting Temp: 575-675oF (302-357oC)

 Recommended Use

   Recommended Use
 ● Soft Boutique.    ● Soft Boutique.

 Industry Equivalents

   Industry Equivalents
 ● Atlas 5632    ● Conquest NC-36A
         

 #36

   36M
 COMPOSITION: Tin (Sn) 36%    COMPOSITION: Tin (Sn) 36%
Antimony (Sb) 3%   Antimony (Sb) 3%
Lead (Pb) 58%   Lead (Pb) 59%
Cadmium (Cd) 3%   Cadmium (Cd) 2%

 Density: 0.3487 Lbs/in3 (9.67 g/cm3)

   Density: 0.3496 Lbs/in3 (9.69 g/cm3)
 Casting Temp: 500-550oF (260-288oC)    Casting Temp: 500-565oF (260-296oC)

 Recommended Use

   Recommended Use
 ● Cost effective jewelry.    ● Soft Boutique.

 Industry Equivalents

   Industry Equivalents
 ● AIM 36, Canfield CAD-36    ● Hirsch 36CDM
         

 36BH

   36W
 COMPOSITION: Tin (Sn) 36%    COMPOSITION: Tin (Sn) 36%
Antimony (Sb) 3%   Antimony (Sb) 3%
Lead (Pb) 60%   Lead (Pb) 61%
Cadmium (Cd) 1%    

 Density: 0.3506 Lbs/in3 (9.72 g/cm3)

   Density: 0.3516 Lbs/in3 (9.75 g/cm3)
 Casting Temp: 500-575oF (260-302oC)    Casting Temp: 575-675oF (302-357oC)

 Recommended Use

   Recommended Use
 ● Cost effective jewelry.    ● Soft Boutique.

 Industry Equivalents

   Industry Equivalents
 ● AIM 36LC , Conquest NC-36BH    ● Aim 36W, Canfield J-363, Conquest NC-36, Hirsch 363
         

 #365

   Special "A"
 COMPOSITION: Tin (Sn) 36%    COMPOSITION: Tin (Sn) 38%
Antimony (Sb) 5%   Antimony (Sb) 3%
Lead (Pb) 59%   Lead (Pb) 59%

 Density: 0.3482 Lbs/in3 (9.65 g/cm3)

   Density: 0.3487 Lbs/in3 (9.67 g/cm3)
 Casting Temp: 575-675oF (302-357oC)    Casting Temp: 575-675oF (302-357oC)

 Recommended Use

   Recommended Use
 ● Soft Boutique.    ● Soft Boutique.

 Industry Equivalents

   Industry Equivalents
 ● Canfield J-365, Hirsch 365    ● CMC Special A
         

 #60

   #68
 COMPOSITION: Tin (Sn) 60%    COMPOSITION: Tin (Sn) 68%
Antimony (Sb) 3%   Antimony (Sb) 6%
Lead (Pb) 37%   Lead (Pb) 23%
    Cadmium (Cd) 3%

 Density: 0.3166 Lbs/in3 (8.77g/cm3)

   Density: 0.2969 Lbs/in3 (8.22 g/cm3)
 Casting Temp: 500-600oF (260-316oC)    Casting Temp: 500-600oF (260-316oC)

 Recommended Use

   Recommended Use
 ● Textured Pieces.    ● Textured Pieces.

 Industry Equivalents

   Industry Equivalents
 ● Atlas 7604    ● AIM 77
         

 70BH

   70M
 COMPOSITION: Tin (Sn) 70%    COMPOSITION: Tin (Sn) 70%
Antimony (Sb) 5%   Antimony (Sb) 6%
Lead (Pb) 24%   Lead (Pb) 21%
Copper (Cu) 1%   Cadmium (Cd) 3%

 Density: 0.2977 Lbs/in3 (8.25 g/cm3)

   Density: 0.2940 Lbs/in3 (8.14 g/cm3)
 Casting Temp: 500-600oF (260-316oC)    Casting Temp: 500-600oF (260-316oC)

 Recommended Use

   Recommended Use
 ● Textured Pieces.    ● Textured Pieces.

 Industry Equivalents

   Industry Equivalents
 ● Canfield J-570 , Conquest NC-70BH    ● Hirsch 70CDM
         

 #70

   85M
 COMPOSITION: Tin (Sn) 70%    COMPOSITION: Tin (Sn) 85%
Antimony (Sb) 6%   Antimony (Sb) 3%
Lead (Pb) 24%   Lead (Pb) 10%

 Density: 0.2969 Lbs/in3 (8.22 g/cm3)

   Density: 0.2871 Lbs/in3 (7.70 g/cm3)
 Casting Temp: 500-600oF (260-316oC)    Casting Temp: 525-600oF (274-316oC)

 Recommended Use

   Recommended Use
 ● Textured Pieces.    ● Tailored/Filigree.

 Industry Equivalents

   Industry Equivalents
 ● AIM 70, Conquest NC-77, Hirsch 706    ● Canfield CAD-85, Hirsch 85CDM
         

 88M

   #881
 COMPOSITION: Tin (Sn) 88%    COMPOSITION: Tin (Sn) 88%
Antimony (Sb) 1.5%   Antimony (Sb) 1.5%
Lead (Pb) 9%   Lead (Pb) 10%
Cadmium (Cd) 1.5%   Cadmium (Cd) 0.5%

 Density: 0.2768 Lbs/in3 (7.67g/cm3)

   Density: 0.2778 Lbs/in3 (7.69 g/cm3)
 Casting Temp: 525-600oF (274-316oC)    Casting Temp: 525-600oF (274-316oC)

 Recommended Use

   Recommended Use
 ● Tailored/Filigree.    ● Tailored/Filigree.

 Industry Equivalents

   Industry Equivalents
 ● Hirsch 88CDM    ● Hirsch 88M
         

 #882

   #886
 COMPOSITION: Tin (Sn) 88%    COMPOSITION: Tin (Sn) 88%
Antimony (Sb) 2%   Antimony (Sb) 6%
Lead (Pb) 8%   Lead (Pb) 6%
Cadmium (Cd) 2%    

 Density: 0.2755 Lbs/in3 (7.63 g/cm3)

   Density: 0.2706 Lbs/in3 (7.49 g/cm3)
 Casting Temp: 525-600oF (274-316oC)    Casting Temp: 525-600oF (274-316oC)

 Recommended Use

   Recommended Use
 ● Filigree/Fashion work.    ● Filigree/Fashion work.

 Industry Equivalents

   Industry Equivalents
 ● Canfield CAD-88    ● Conquest NC-88
         

 88SP

   88S
 COMPOSITION: Tin (Sn) 88.5%    COMPOSITION: Tin (Sn) 88.5%
Antimony (Sb) 1.5%   Antimony (Sb) 2.5%
Lead (Pb) 8.5%   Lead (Pb) 8.5%
Cadmium (Cd) 1.5%   Cadmium (Cd) 0.5%

 Density: 0.2761 Lbs/in3 (7.65 g/cm3)

   Density: 0.2753 Lbs/in3 (7.63 g/cm3)
 Casting Temp: 450-550oF (232-288oC)    Casting Temp: 500-550oF (260-288oC)

 Recommended Use

   Recommended Use
 ● Filigree/Fashion work.    ● Fashion pieces.

 Industry Equivalents

   Industry Equivalents
 ● AIM SPKP    ● AIM 88.5, Canfield SX-88
         

 88W

   #902
 COMPOSITION: Tin (Sn) 88.5%    COMPOSITION: Tin (Sn) 905%
Antimony (Sb) 2.5%   Antimony (Sb) 2%
Lead (Pb) 9%   Lead (Pb) 6%
    Cadmium (Cd) 2%

 Density: 0.2753 Lbs/in3 (7.63g/cm3)

   Density: 0.2726 Lbs/in3 (7.55 g/cm3)
 Casting Temp: 500-550oF (260-288oC)    Casting Temp: 500-575oF (260-302oC)

 Recommended Use

   Recommended Use
 ● Fashion pieces.    ● Filigree/Fashion work.

 Industry Equivalents

   Industry Equivalents
 ● AIM 88W    ● Atlas 79010
         

 #90

   #92
 COMPOSITION: Tin (Sn) 90%    COMPOSITION: Tin (Sn) 92%
Antimony (Sb) 2%   Antimony (Sb) 3%
Lead (Pb) 8%   Lead (Pb) 5%

 Density: 0.2745 Lbs/in3 (7.60 g/cm3)

   Density: 0.2699 Lbs/in3 (7.47 g/cm3)
 Casting Temp: 500-575oF (260-302oC)    Casting Temp: 475-525oF (246-274oC)

 Recommended Use

   Recommended Use
 ● Tailored/Filigree.    ● Filigree/Fashion work.

 Industry Equivalents

   Industry Equivalents
 ● Hirsch 90    ● AIM 92
         

 9A

   J44
 COMPOSITION: Tin (Sn) 92%    COMPOSITION: Tin (Sn) 92%
Antimony (Sb) 3.5%   Antimony (Sb) 4%
Lead (Pb) 4%   Lead (Pb) 4%
Cadmium (Cd) 0.5%    

 Density: 0.2685 Lbs/in3 (7.44 g/cm3)

   Density: 0.2682 Lbs/in3 (7.43 g/cm3)
 Casting Temp: 475-525oF (246-274oC)    Casting Temp: 475-525oF (246-274oC)

 Recommended Use

   Recommended Use
 ● Filigree/Fashion work.    ● Tailored/Filigree.

 Industry Equivalents

   Industry Equivalents
 ● Conquest NC-9A    ● Atlas 7924, Canfield J-44, Conquest NC-9, Hirsch 9244
         

 93M

   #932
 COMPOSITION: Tin (Sn) 93%    COMPOSITION: Tin (Sn) 93%
Antimony (Sb) 1.5%   Antimony (Sb) 2%
Lead (Pb) 4%   Lead (Pb) 5%
Cadmium (Cd) 1.5%    

 Density: 0.2695 Lbs/in3 (7.46g/cm3)

   Density: 0.2701 Lbs/in3 (7.48 g/cm3)
 Casting Temp: 450-500oF (232-260oC)    Casting Temp: 475-525oF (246-274oC)

 Recommended Use

   Recommended Use
 ● Filigree/Fashion work.    ● Filigree/Fashion work.

 Industry Equivalents

   Industry Equivalents
 ● AIM 931, Canfield CAD-93, Hirsch 93CDM    ● AIM NM, Canfield 93-L, Hirsch 93L
         

 J Alloy

   #932
 COMPOSITION: Tin (Sn) 93.5%    COMPOSITION: Tin (Sn) 95%
Antimony (Sb) 1.5%   Antimony (Sb) 2%
Lead (Pb) 3.5%   Lead (Pb) 3%
Cadmium (Cd) 1.5%    

 Density: 0.2688 Lbs/in3 (7.44 g/cm3)

   Density: 0.2672 Lbs/in3 (7.40 g/cm3)
 Casting Temp: 475-525oF (246-274oC)    Casting Temp: 475-525oF (246-274oC)

 Recommended Use

   Recommended Use
 ● Filigree/Fashion work.    ● Tailored/Filigree.

 Industry Equivalents

   Industry Equivalents
 ● CMC J Alloy    ● Hirsch 95

© 2001-2011 Alchemy Castings (1464012 Ontario Inc.) & Alchemy Art Lead Products (1464013 Ontario Inc.)

563 Kenilworth Ave. N., Hamilton, Ontario, Canada L8H 4T8
Toll-Free: 1-866-312-9084, Phone: (905) 312-9084, Fax: (905) 312-9085,
Email